Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styron CALIBREâ„¢ 2061-22 Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Styron
Trade Name CALIBRE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron CALIBREâ„¢ 2061-22 Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CALIBREâ„¢ 2061-22 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and temperatures.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.15 %
0.15 %
23°C, 24hrs; ASTM D570
Water Absorption at Saturation 0.32 %
0.32 %
23°C, 50% RH; ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 22 g/10 min

@Load 1.20 kg,
Temperature 300 °C
22 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 73
73
ASTM D785
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Ultimate 65.5 MPa
9500 psi
50 mm/min; ASTM D638
Tensile Strength, Yield 60.0 MPa
8700 psi
50 mm/min; ASTM D638
Elongation at Break 120 %
120 %
50 mm/min; ASTM D638
Tensile Modulus 2.34 GPa
340 ksi
50 mm/min; ASTM D638
Flexural Strength 96.5 MPa
14000 psi
3-points, 2 mm/min; ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
3-points, 2 mm/min; ASTM D790
Izod Impact, Notched 7.47 J/cm
14.0 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Tensile Impact 96.1 J/cm
180 ft-lb/in
ASTM D1822
Dart Drop, Total Energy 72.0 J
53.1 ft-lb
8000 ipm; ASTM D3763
Abrasion 45
45
[%] Taber Abrasion Resistance - Δ; ASTM D1044
Thermal Properties Metric English Comments
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 142 °C
288 °F
annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
258 °F
unannealed; ASTM D648
139 °C
282 °F
annealed; ASTM D648
Vicat Softening Point 152 °C
306 °F
50°C/hr, 50N; ASTM D1525
Optical Properties Metric English Comments
Refractive Index 1.586
1.586
ASTM D542
Haze 1.0 %
1.0 %
ASTM D1003
Transmission, Visible 89 %
89 %
ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Dielectric Constant 3.0

@Frequency 60 Hz
3.0

@Frequency 60 Hz
ASTM D150
3.0

@Frequency 1e+6 Hz
3.0

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 16.5 kV/mm
420 kV/in
ASTM D149
Dissipation Factor 0.0010

@Frequency 60 Hz
0.0010

@Frequency 60 Hz
ASTM D150
0.0020

@Frequency 1e+6 Hz
0.0020

@Frequency 1e+6 Hz
ASTM D150
Users viewing this material also viewed the following: