Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 2.34 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.34 GPa
339 ksi
51 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
Tensile Modulus 2.34 GPa
339 ksi
Type I, 51 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Molding M5700 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
Tensile Modulus 2.34 GPa
339 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer
Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ..
Tensile Modulus 2.34 GPa
339 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Asia Pacific)
Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ..
Tensile Modulus 2.34 GPa
339 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ..
Tensile Modulus 2.34 GPa
339 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer
Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch..
Tensile Modulus 2.34 GPa
339 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Lexan® FXE144H PC (Asia Pacific)
FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe..
Tensile Modulus 2.34 GPa
339 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® ML6031 PC Copolymer (Asia Pacific)
High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacific ..
Tensile Modulus 2.34 GPa
339 ksi
Type I, 51 mm/min; ASTM D638
PolyOne Geon™ HTX M6230 Polyvinyl Chloride Alloy (PVC Alloy)
Information provided by PolyOne
Tensile Modulus 2.34 GPa
339 ksi
ASTM Data
Americas Styrenics Styron® XL-8023VC High Impact Polystyrene  (discontinued **)
STYRON® XL-8023 VC high impact polystyrene is designed to provide molders of VCR cassettes with the impact and gloss they require, at economics and processability highly advantaged over ABS resins...
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
Solvay Specialty Polymers Supradel® HTS-2600 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2600 is a high-temperature, high-performance, amorphous, sulfone polymer. In addition to exceptional thermal performance, this resin has the other performance features and attributes t..
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
LG Chemical Lupoy 1301EP22 Polycarbonate Resin
Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
LG Chemical Lupoy 1302HP-21 Polycarbonate Resin
Description: LUPOY PC 1302HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
LG Chemical Lupoy 1303-15 Polycarbonate Resin
Description: LUPOY PC 1303-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Tensile Modulus 2.34 GPa

@Thickness 3.18 mm
339 ksi

@Thickness 0.125 in
ASTM D638
Solvay Specialty Polymers Radel® R-5800 Polyphenylsulfone (PPSU)
Radel® R-5800 is a high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer exceptiona..
Tensile Modulus 2.34 GPa
339 ksi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ 201-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 201-15 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc..
Tensile Modulus 2.34 GPa
339 ksi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ 201-22 Polycarbonate Resin
Overview: CALIBREâ„¢ 201-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc..
Tensile Modulus 2.34 GPa
339 ksi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ 203-22 Polycarbonate Resin
Overview: CALIBREâ„¢ 200-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc..
Tensile Modulus 2.34 GPa
340 ksi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ 2061-22 Polycarbonate
CALIBREâ„¢ 2061-22 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and..
Tensile Modulus 2.34 GPa
339 ksi
50 mm/min; ISO 527-2/50; ASTM D638
Styron CALIBREâ„¢ 2061-22 Polycarbonate Resin
Overview: CALIBREâ„¢ 2061-22 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-22 provides exceptional clarity, heat resistance, impa..
Tensile Modulus 2.34 GPa
340 ksi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 4330-22 Polycarbonate
EMERGEâ„¢ PC 4330-22 advanced resin is high-performance polycarbonate resin offering ultraviolet light stability, high heat resistance, toughness, and superior flow. Applications: Consumer Elec..
Tensile Modulus 2.34 GPa
340 ksi
2 in/min; ASTM D638
Styron CALIBREâ„¢ 201-15 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Modulus 2.34 GPa
339 ksi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ 302EP-22 Polycarbonate Resin
Overview: CALIBREâ„¢ 300EP-22 Series are polycarbonate resins that offer exceptional impact resistance, heat distortion resistance and optical clarity for injection molding applications. Their hi..
Tensile Modulus 2.34 GPa
339 ksi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ MEGARAD 2081-6LR Polycarbonate Resin
Overview: CALIBREâ„¢ 2081-6LR Polycarbonate resin was developed for medical applications requiring improved resistance to lipids over standard polycarbonate resins. When exposed to a 20% intralip..
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
Westlake Plastics Radel® R 4400 Polyphenylsulfone For Medical Applications
Medical grade Radel R4400 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability,..
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
Westlake Plastics Radel® R 5500 Polyphenylsulfone
Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness, and good environmental stress c..
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU)
RADEL® R is a Polyphenysulfone produced by Solvay Advanced Polymers. RADEL® R is in the same performance category as products like Polysulfone and ULTEM® (PEI). RADEL® R has increased performa..
Tensile Modulus 2.34 GPa
339 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Lexan® FXE144H PC (Europe-Africa-Middle East)
FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe..
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
PolyOne Lubri-Tech™ 5209 S2 Natural A Acetal Copolymer, 9 Melt with Silicone  (discontinued **)
Information provided by PolyOne™ Corporation