Material Notes:
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming.MAGNUM® 9043 ABS resin is a high gloss sheet extrusion grade tailored for refrigerator liner applications.Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM Data
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
Melt Flow 2.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
2.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ASTM Data
Tensile Strength, Yield 38.6 MPa
5600 psi
ASTM Data
Elongation at Break 40 %
40 %
ASTM Data
Tensile Modulus 2.10 GPa
305 ksi
ASTM Data
Izod Impact, Notched 4.80 J/cm
8.99 ft-lb/in
ASTM Data
Impact Test 54.0 J

@Temperature 23.0 °C
39.8 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
Unannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
Unannealed; ASTM Data
Vicat Softening Point 107 °C
225 °F
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
Optical Properties Metric English Comments
Gloss 95 %
95 %
Gardner Gloss, 60°
Users viewing this material also viewed the following: