Material Notes:
Chemical Name: Poly[[6-[(1,1,3,3-tetramethylbutyl)amino]-1,3,5-triazine-2,4-diyl][(2,2,6,6-tetramethyl-4-piperidinyl)imino]-1,6-exanediyl[(2,2,6,6-tetramethyl-4-piperidinyl imino]])Characterization: Ligh stabilizer 791 is a synergistic mixture of Light stabilizer 944 and Light stabilizer 770. It is an excellent UV stabilizer especially for PP thick sections, which offers excellent surface protection. It also shows high stabilization efficiency in PP tapes.Applications: Light stabilizer 791 areas of application are PP, PP/EPDM and PP/PE/EPDM blend(TPO's).Features/benefits: Light stabilizer 791 is an excellent UV stabilizer for thick sections, e.g. automotive bumpers, fascia, garden furniture etc. The synergism between the high and low molecular weight HALS components of Light stabilizer 791 guarantees maximum protection for the polymer against degradation from UV radiation and long-term heat exposure.Information Provided by Suqian Unitechem Co., Ltd.
Physical Properties Metric English Comments
Density 1.00 - 1.20 g/cc
0.0361 - 0.0434 lb/in³
Relative density
Molecular Weight 481 g/mol
481 g/mol
Vapor Pressure <= 1.00e-7 bar

@Temperature 20.0 °C
<= 0.0000750 torr

@Temperature 68.0 °F
Thermal Properties Metric English Comments
Melting Point >= 50.0 °C
>= 122 °F
Descriptive Properties Value Comments
Appearance White or slightly yellowish solid