Material Notes:
Hiprolon® 400 NN is a medium viscosity specialty polyamide. Features: low density, low water absorption, high dimension stability, high notched impact resistance in large temperature ranges, and good chemical resistance. It is widely used as a neat resin for compounding, general injection molding process, tubing or film extrusion, and powder coating et al.Information provided by Suzhou Hipro Polymers Co. Ltd
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ISO 1183
Water Absorption 0.45 %
0.45 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-2/1A
Tensile Modulus 1.10 GPa
160 ksi
ISO 527-1/-2
Flexural Modulus 1.10 GPa
160 ksi
ISO 178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
1.40 J/cm²

@Temperature 23.0 °C
6.66 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 190 °C
374 °F
ISO 11357-1/-2
Users viewing this material also viewed the following: