Sylvin Technologies 5123 PVC Wire/Cable Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Sylvin Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sylvin Technologies 5123 PVC Wire/Cable Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
10 seconds
Tensile Strength, Ultimate 16.5 MPa
2400 psi
Elongation at Break 380 %
380 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air <= 75.0 °C
<= 167 °F
Brittleness Temperature -44.0 °C
-47.2 °F
Oxygen Index 21.2 %
21.2 %
Processing Properties Metric English Comments
Processing Temperature 163 - 174 °C
325 - 345 °F
Recommended Stock Temperature