Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 75.0 °C | 167 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable JAC32A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable JJX20A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable JLK51L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable MJF114A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable WJJC34L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable WJJX207L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | Short Term Use |
Polycasa XT 610 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | Continuous; FRISETTA Test Method |
Nilit RECONYL B S Recycled nylon 6 for injection molding Recycled nylon 6 for injection molding, impact modified (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | Continuous (GTP 50% Tensile); IEC 60216 |
PolyOne Bergamid™ B700 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | Continuous (GTP 50% Tensile); IEC 60216 |
PolyOne Bergamid™ B700 X2 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | Continuous; FRISETTA Test Method |
Nilit RECONYL B S20 Recycled nylon 6 for injection molding Recycled nylon 6 for injection molding, impact modified (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 75.0 - 90.0 °C | 167 - 194 °F | Average value: 86.0 °C Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | |
Permabond 932 Cyanoacrylate PERMABOND 932 is a low odor, nonfogging, nonfrosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | 70-80°C (160-175°F) Heat distortion temperature. |
Abatron AboCast 50-3/AboCure 8012-7 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Low-viscosity, like motor oil; Light Amber color; Combines lower viscosity with longer pot life. Shelf life is 12+ months.Processing: 2/1 ratio. Po.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | |
LATI Latan 9 POM Polyoxymethylene (POM). Unfilled. Medium viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | |
Styrolution Terlux® 2802 TR Q434 Transparent MABS Description: Terlux® 2802 TR Q434 is a new grade with enhanced toughness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 97-G0029C-82 Polyvinyl Chloride, Flexible Notes: 80°C Jacket; RoHS CompliantFeatures: Flame Retardant Uses: Cable Jacketing; Communication Wire JacketingAgency Ratings: UL 62; UL 444 Forms: Pellets Processing Method: ExtrusionInformation.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 65012 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 80102 Polyvinyl Chloride, Flexible Notes: 75°C Insulation; RoHS Compliant Uses: InsulationAgency Ratings: UL 1063; UL 1581; UL 62; UL 83 Forms: Pellets Wire Types: TWInformation Provided by Teknor Apex |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | Continuous |
Wolf Kunststoff ZEDEX® ZX-100EL55 A1F Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | Continuous |
Wolf Kunststoff ZEDEX® ZX-100EL63 A1G Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | |
ELASTO UK Dryflex® 400801S SBS Based Material, 80A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | |
ELASTO UK Dryflex® 402601S SBS Based Material, 60A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | |
ELASTO UK Dryflex® 422401S SBS Based Material, 40D Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | |
ELASTO UK Dryflex® 422451S SBS Based Material, 45D Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Maximum Service Temperature, Air | <= 75.0 °C | <= 167 °F | Continuous Use |
Arlon CuClad 6250 Bonding Film Thermoplastic Bonding FilmsSimilar Dk and Df range to many PTFE laminatesBenefits:Can be reheated to remelt and reflow bonding filmExcellent Electrical PropertiesTypical Applications:Stripline Circu.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable W1100 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | ASTM D 3575 |
Eurofoam Porocell POR 300/100 Ethylene Octane Metallocene EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | DIN EN 14706 |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Maximum Service Temperature, Air | 75.0 °C | 167 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable 1721-xx14E Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |