Material Notes:
Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore C 75
75
At 10 seconds
Tensile Strength, Ultimate 20.7 MPa
3000 psi
Elongation at Break 350 %
350 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air <= 105 °C
<= 221 °F
Brittleness Temperature -11.0 °C
12.2 °F
Flammability, UL94 V-1
V-1
VW-1
Oxygen Index 25.6 %
25.6 %
Processing Properties Metric English Comments
Processing Temperature 177 - 191 °C
350 - 375 °F
Recommended Stock Temperature