Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D638-95 |
Multibase Multi-Flex® TPO D-5509 This TPO product is suitable for outdoor applications with good low temperature properties and UV resistance in applications such as ridge vents.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D638-95 |
Multibase Multi-Pro® 0710 C Brown Polypropylene Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D638 |
Multibase Multi-Pro® 1510 CNU White Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D638-95 |
Multibase Multi-Pro® 4013 CU Yellow 40% Filler Content Polypropylene Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D638 |
Multibase Nylex™ 1230 Polyamide + PP Forms: PelletsInformation provided by Multibase |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D638 |
Petromont 1100 High Density Polyethylene Resin Petromont HDPE 1100 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This multi-purpose resin is intended primarily for use in most intermittent and continuous b.. |
|||
Tensile Strength, Ultimate | 20.7 - 96.0 MPa | 3000 - 13900 psi | Average value: 65.0 MPa Grade Count:14 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D4745 |
3M Dyneon™ CC698 PTFE 20% Fiberglass/Carbon Filled
(discontinued **) Product Form: Black, pelletized powder. Applications include valve seats.Data provided by Dyneon. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D882 |
Total PPR 8650 Polypropylene, Random Copolymer ATOFINA 8650 is a low melting, high ethylene random copolymer with improved color, optics and impact properties. The low melting point of ATOFINA 8650 makes it an excellent heat seal layer for orie.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | |
Cytec EN-2532 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D412 |
Dow SPECTRIM™ 35-S Reaction Moldable Polymer SPECTRIM™ 35-S reaction moldable polymer is a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology developed by the Dow Chemical Company.Information p.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D412 |
Dow Tyrin® CM0136 Formulation FormulationTyrin® CPE Elastomer |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D412 |
Dow Tyrin® CM0836 Formulation FormulationTyrin® CPE Elastomer |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D638 |
Colorite Polymers Elastichem 7511TX-02 Vinyl Compound Description: All components in Elastichem are sanctioned by the U.S. Food & Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulations. For medical use, co.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | |
Colorite Polymers Self Frosting™ 9011SF Vinyl Compound Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | |
Colorite Polymers 9011 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | |
Colorite Polymers 9012 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | |
Dymax 3073 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | |
Dymax 628 Structural Adhesive Structural Adhesives for Rugged Bonding, Sealing, Tacking and Potting in SecondsMulti-Cure® 600 Series products are rapid setting adhesives that cure by UV light, activator or heat. These products .. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | Bond strength to glass |
Dymax Light Weld® 402 High Clarity Glass Bonding Adhesive Glass Bonding in SecondsDescriptionDymax Light Weld® 400 Series adhesives form high-clarity, invisible bonds between glass and other substrates in seconds. In addition to many structural glass bond.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D638 |
Arkema Group Solarkote® P-601 Acrylic PVC Capstock, white, high glossInformation provided by Arkema Group |
|||
Tensile Strength, Ultimate | 20.7 - 34.5 MPa | 3000 - 5000 psi | |
Bulk Molding Compounds BMC 700 Thermoset Polyester, High Arc Quench Electrical Grade BMC 700 is a general purpose, mineral filled, glass fiber-reinforced polyester compound that was initially designed for molding arc chutes. It has superior arc quench properties. As with all other B.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D638 |
American Polymers API 645-21 Polystyrene API 645-21 is a super high impact polystyrene used in applications requiring a superior level of toughness along with good tensile and flexural properties. On balance this extrusion grade polymer a.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | TM R050-36 |
Resinlab® EP1296 Highly Filled, Moderately Thixotropic Black Casting Resin Resinlab™ EP1296 is a highly filled, moderately thixotropic black casting resin designed for applications requiring good thermal conductivity, low shrinkage and a low CTE. It was especially formula.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® 4085 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound
(disc Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont .. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D412 |
MF-5001 Polyurethane-based Biomedical Elastomer |