Material Notes:
Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
10 seconds
Tensile Strength, Ultimate 11.0 MPa
1600 psi
Elongation at Break 480 %
480 %
Tear Strength Test 225
225
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 157 - 168 °C
315 - 335 °F