Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 11.0 MPa | >= 1600 psi | ASTM D638-95 |
Multibase Multi-Flex® TPO 4107 BLK Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
3M Dyneon™ Fluorel™ FE-5830Q Fluoroelastomer VF2 + HFP + TFE Terpolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 70.5%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. 70.5% F grade terpolymer with best pe.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
ExxonMobil Optema® TC-113 Ethylene Methyl Acrylate for Compounding
(discontinued **) Data provided by the manufacturer, Exxon Chemical.23.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used as an impact modifier or compatibilizer in polymer compounds. It ca.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Chevron Phillips KN 226B LDPE Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; Mold Release Agent Added; ASTM D 4976 Classification: PE 112, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Excellent Mold Release, Mode.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Chevron Phillips Marlex® 1409 Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Excellent Warping Resistance, Excellent Mold Release, Moderate ESCRApplications.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | 500 mm/min (20 in./min.); ASTM D638, Type IV Specimen |
Eastman 1550P Polyethylene
(discontinued **) Injection molding gradeUnless otherwise noted, all tests are run at 23°C and 50% RH. Where required, samples are compression molded per ASTM D1928.Information from manufacturer data sheet.Eastman .. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Huntsman PE 1017 Film Extrusion Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, and FDA compliant.Features: Good impact strength, good machinability, heat seal and foaming characteristicsApplications: Film Extrusion: industrial line.. |
|||
Tensile Strength, Ultimate | 11.0 - 75.8 MPa | 1600 - 11000 psi | Average value: 41.7 MPa Grade Count:25 |
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Sylvin Technologies 8950-70 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Sylvin Technologies 8999-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Sylvin Technologies 9600-65 Clear PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Sylvin Technologies 9950-70 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Westlake EC483 Low Density Polyethylene WESTLAKE low-density polyethylene EC483 is recommended for use in the boardstock coating industry. This resin has low neck-in, good heat sealing properties, and good drawdown characteristics.Applica.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Covestro Baydur® 40 Polyurethane Rigid integral skin polyurethane foam for lightweight moldings. Sandwich structure gives a high stiffness-to-weight ratio.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience .. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Cytec EN-2523 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Cytec EN-2541 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Dow DOWLEX™ IP-41 High Density Polyethylene DOWLEX® IP-41 resin is an improved processing high density polyethylene resin designed to offer excellent processability and rigidity required for food containers, overcaps, and other general purpo.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Dow HDPE 38152M High Density Polyethylene DOW HDPE 38152M resin is a medium molecular weight distribution copolymer designed to offer good impact strength and stress crack resistance with excellent toughness. This resin has excellent proces.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4570 Dense Extruded Profile FormulationNordel® IP 4570 |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D412 |
Colorite Polymers Weatherflex™ CS1534WX (NTL01P) Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Colorite Polymers 92-623A General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 4680 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 4680 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Colorite Polymers 6574 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Huntsman PE1059 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down and good processability.Applications: Film extrusion: non-abrasive packaging applications.FDA Notes: Conforms to FDA regulation 21 CFR 177.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Huntsman PE2030 Injection Molding Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, and FDA compliant.Features: High mechanical flexing properties, excellent processability, good stress crack resistance, and very good low temperature st.. |
|||
Tensile Strength, Ultimate | 11.0 - 14.0 MPa | 1600 - 2030 psi | Average value: 12.5 MPa Grade Count:4 |
Overview of materials for Low Density Polyethylene (LDPE), Sheet/Profile extrusions This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Sheet/Profile extrusions". Each property range of values reported is mi.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | TM R050-36 |
Resinlab® EP1290 Gray Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Gray is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to m.. |
|||
Tensile Strength, Ultimate | 11.0 - 28.0 MPa | 1600 - 4060 psi | Average value: 20.4 MPa Grade Count:30 |
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |