Trade Name Porene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TPI Porene® GA800TW High Gloss/Weather Resistant/Antistatic Grade ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
INJECTION MOLDING; ANTISTATIC; WEATHER RESISTANT. HOUSING OF ELECTRICAL APPLIANCES, e.g. ELECTRIC FAN, TELEPHONE, CALCULATOR, TOYSPorene® is a registered trademark of Thai Petrochemical Industry Co. LTD. Information provided by Dayson Polymers.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Melt Flow 20 g/10 min

@Load 10.0 kg,
Temperature 220 °C
20 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
0.250 inch; ASTM D785
Tensile Strength at Break 52.0 MPa
7540 psi
ASTM D638
Flexural Yield Strength 70.60 MPa
10240 psi
ASTM D790
Flexural Modulus 2.35 GPa
341 ksi
ASTM D790
Izod Impact, Notched 3.32 J/cm
6.21 ft-lb/in
0.250 inches; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °C
205 °F
0.250 inch; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.2 °C
189 °F
0.250 inches; ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Melt Temperature 190 - 240 °C
374 - 464 °F