Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 1012 C Polypropylene Calcium Carbonate Filler, 12% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 2514 XU Polypropylene Mineral Filled, 25% by weight.Features:Heat Resistance, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureTable ProductsInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C @Thickness 3.18 mm |
205 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Maxxam™ FR PP 401 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C @Thickness 3.18 mm |
205 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Maxxam™ PPC-40C Nat Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C @Thickness 3.18 mm |
205 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Maxxam™ XN-418.G001-1000 Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D648 |
RheTech Products HP513-01 High Stiffness Polypropylene Copolymer, Medium Impact, UV Stabilized, Black Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 2510 XG Polypropylene Mineral Filled, 25% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D648 |
RheTech Products HP513-538UV High Stiffness Polypropylene Copolymer, UV Stabilized, W12A 848 Black Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D648 |
Global CPP-110 10% CaC03 Filled Polypropylene Information provided by Global Polymers Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D648 |
Global GPP-2500 Polypropylene Impact Copolymer, Nucleated Information provided by Global Polymers Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Techmer ES Statiblend® HDPE C BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveUL File Number: E157318Appearance: BlackTPCI# 9411115Information provided by TP Composites.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Techmer ES Statiblend® HIPS E Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and ConductiveAppearance: Natural ColorProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM Data |
Styron Magnum™ 344CC ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM Data |
Styron Magnum™ 780HP ABS, High Heat, High Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® HIPS 1000 FR-E Availability: North AmericaForms: PelletsFeatures: Flame RetardantRoHS Compliance: RoHS CompliantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® HIPS FR-1 Availability: North AmericaForms: PelletsFeatures: Flame RetardantRoHS Compliance: RoHS CompliantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PP FR-N X Availability: North AmericaForms: PelletsFeatures: Flame Retardant Appearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PP FR-N X BKN001 Availability: North AmericaForms: PelletsFeatures: Flame Retardant Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® HIPS E SL5 Availability: North AmericaForms: PelletsAdditive: Silicone Lubricant (5%)Appearance: Natural ColorProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Styron EMERGEâ„¢ 7700 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7700 Advanced Resin is an ignition-resistant PC/ABS blend that contains no chlorine for bromine additives. It has superior processability for injection molding applicat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM Data |
Styron Magnum™ 344HP ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D-648 |
Axiall HHP-190 Rigid PVC, Extrusion Georgia Gulf HHP-190 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Heat Resistance & Thermal StabilityImpact Strength & ToughnessDimensi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D648 |
Americas Styrenics STYRON® 675 High Heat Crystal Polystyrene Product CharacteristicsHigh heatMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsThin-walled partsInformation provided by AmericasStyrenics LLC. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 - 205 °C | 205 - 401 °F | Average value: 149 °C Grade Count:153 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |