TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR Sulfur

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR Sulfur.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Like many oil resistant synthetic rubbers, Millathane 76 requires a treated grade of sulfur to ensure proper dispersion.All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
Tensile Strength, Yield 33.45 MPa
4852 psi
Elongation at Yield 562 %
562 %
100% Modulus 0.00394 GPa
0.571 ksi
200% Modulus 0.008915 GPa
1.293 ksi
300% Modulus 0.01546 GPa
2.243 ksi
Tear Strength 61.8 kN/m
353 pli
Die C
Compression Set 38.4 %

@Temperature 70.0 °C,
Time 79200 sec
38.4 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 8.00 min

@Temperature 155 °C
0.133 hour

@Temperature 311 °F
TC90