Tear Strength 61.8 kN/m
353 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N650 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 61.8 kN/m
353 pli
ASTM D624
SK Chemicals SKYTHANE® UB400 Hotmelt Lamination Film
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta..
Tear Strength 61.8 kN/m
353 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR Sulfur
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man..
Tear Strength 61.8 kN/m
353 pli
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Translink 555
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 61.8 kN/m
353 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N650 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 61.8 kN/m
353 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR Sulfur
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man..
Tear Strength 61.8 kN/m
353 pli
ASTM D624
SK Chemicals SKYTHANE® 400 Hotmelt Grade UB Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tear Strength 61.8 kN/m
353 pli
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Translink 555
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..