Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Precipitated Calcium Carbonate

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Precipitated Calcium Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Zinc Stearate0.5Poly AC 617A1.0MBTS4.0MBT2.0Thanecure® ZM1.0TP-9510.0Sulfur2.0Precipitated Calcium Carbonate60All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength, Yield 20.12 MPa
2918 psi
Elongation at Yield 721 %
721 %
100% Modulus 0.00157 GPa
0.228 ksi
200% Modulus 0.00197 GPa
0.285 ksi
300% Modulus 0.00255 GPa
0.370 ksi
Tear Strength 21.9 kN/m
125 pli
Taber Abrasion, mg/1000 Cycles 41

@Load 1.00 kg
41

@Load 2.20 lb
H-18 wheel
Compression Set 52.7 %

@Temperature 70.0 °C,
Time 79200 sec
52.7 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 155 °C
0.167 hour

@Temperature 311 °F