Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00255 GPa | 0.370 ksi | Typical properties of film cast from toluene solution.; ASTM D412 |
Kraton® D1193 P (SIS) Linear Triblock Copolymer Description: Kraton D1193 P is a clear, linear triblock copolymer based on styrene and isoprene, with a polystyrene content of 24%. It is supplied from North America in the physical form identified:.. |
|||
300% Modulus | 0.00255 GPa | 0.370 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Precipitated Calcium Carbonate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.00255 GPa | 0.370 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Precipitated Calcium Carbonate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |