TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Black Peroxide Cure

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Black Peroxide Cure.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Stearic Acid0.5SR 35010.0N-33050.0AC Poly 617A1.0Di-Cup 40C3.0All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
Tensile Strength, Yield 21.79 MPa
3161 psi
Elongation at Yield 201 %
201 %
100% Modulus 0.01136 GPa
1.648 ksi
200% Modulus 0.02147 GPa
3.114 ksi
Tear Strength 44.5 kN/m
254 pli
Die C
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 155 °C
0.250 hour

@Temperature 311 °F