TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Mistron Vapor Filler

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Mistron Vapor Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subjected to high wear in service. It has a unique combination of excellent properties, such as low temperature characteristics, and resistance to heat deterioration, ozone cracking, weathering and swelling in oils or solvents.FormulationMillathane CM 100.0Mistron Vapor90.0Coumarone-Indene Resin30.0MBTS4.0MBT1.0Sulfur0.75CAYTUR 40.35Zinc Stearate0.50All information provided by TSE Industries
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
Mooney Viscosity 12

@Temperature 121 °C
12

@Temperature 250 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 73
73
Tensile Strength, Yield 20.7 MPa
3000 psi
Elongation at Yield 650 %
650 %
100% Modulus 0.00534 GPa
0.775 ksi
300% Modulus 0.00965 GPa
1.40 ksi
Tear Strength 44.6 kN/m
254 pli
Graves
Compression Set 43 %
43 %
Method B
Processing Properties Metric English Comments
Cure Time 90.0 min

@Temperature 142 °C
1.50 hour

@Temperature 287 °F