Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Taiwan PU Corporation CPU-69-A/B Mixing Ratio 100/42 Polyurethane Casting Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer Taiwan PU Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation CPU-69-A/B Mixing Ratio 100/42 Polyurethane Casting Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Compound of CPU-69-A/B with a mixing ratio of 100/42.Information provided by Taiwan PU Corporation.MatWeb has a separate entry for the unmixed A nd B components.
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
Tensile Strength at Break 15.2 MPa
2200 psi
Elongation at Break 225 %
225 %
Tear Strength 36.3 kN/m
207 pli
Descriptive Properties Value Comments
Mixing Ratio 100/42