Taiwan PU Corporation CPU-69-A/B Polyurethane Casting Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer Taiwan PU Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation CPU-69-A/B Polyurethane Casting Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CPU-69-A consists of polyether polyols and other additives. CPU-69-b is an isocyanate prepolymer. Together they create compounds that cure under room temperature and have short working times, short curing times, good transparency, and adjustable color.Information provided by Taiwan PU Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.05 - 1.09 g/cc
1.05 - 1.09 g/cc
A component
1.08 - 1.12 g/cc
1.08 - 1.12 g/cc
B component
Viscosity 200 - 400 cP

@Temperature 40.0 °C
200 - 400 cP

@Temperature 104 °F
B component
400 - 800 cP

@Temperature 40.0 °C
400 - 800 cP

@Temperature 104 °F
A component
Processing Properties Metric English Comments
Processing Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Both A and B components
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
A and B components
Descriptive Properties Value Comments
Color Brown/yellowish clear liquid
A component
Slightly yellowish or colorless clear liquid
B component
Vacuuming Time 30 min
B component
60 min
A component