Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom PLASTALEN® EH 91 N Polyethylene HDPE regrind for injection molding. General use in all industry branches. Delivered in blue ( approx. RAL 5015) mode.Information Provided by Plastcom spol. s r.o. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom SLOVALEN PC 78 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 - 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with.. |
|||
Mold Temperature | 40.0 - 50.0 °C | 104 - 122 °F | |
Plastcom SLOVALEN PC 81 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom SLOVALEN PH 91 N PP, basic type FeaturesCompounded homopolymer PP. General use in all industry branches. Packing material, garden flower-pots, toys, furniture industry, guides, dowels, clamps, office chairs, holders etc. Delivered.. |
|||
Mold Temperature | 40.0 - 50.0 °C | 104 - 122 °F | |
Plastcom SLOVALEN PQ 81 T 30 PP, 30% mineral filling FeaturesModified PP for injection moulding with the content of 30% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene.. |
|||
Mold Temperature | 16.0 - 50.0 °C | 60.8 - 122 °F | |
PolyOne Maxxam™ PPC-10G Black Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Mold Temperature | 16.0 - 50.0 °C | 60.8 - 122 °F | |
PolyOne Maxxam™ PPC-40T Nat Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Mold Temperature | 16.0 - 50.0 °C | 60.8 - 122 °F | |
PolyOne Maxxam™ PPR-40G Black Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Premix Thermoplastics PRE-ELEC® TPE 1503 Conductive Thermoplastic Compound PRE-ELEC® TPE 1503 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Polykemi AB POLYfill PPH 30030DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Mold Temperature | 25.0 - 50.0 °C | 77.0 - 122 °F | |
Huntsman AVALON® 60 DE Thermoplastic Polyurethane Introduction: AVALON 60 DE is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DE is part of the AVALON Perform Range and offers a premium soling materi.. |
|||
Mold Temperature | 25.0 - 50.0 °C | 77.0 - 122 °F | |
Huntsman AVALON® 85 ABR Thermoplastic Polyurethane Introduction: AVALON 85 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABR is part of the AVALON Performance Range and offers a premium soling .. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | Injection Molding |
LG Chemical KEYFLEX BT 3047D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Mold Temperature | 25.0 - 50.0 °C | 77.0 - 122 °F | |
Huntsman AVALON® 65 DEU Thermoplastic Polyurethane Introduction: AVALON 65 DEU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 65 DEU is part of the AVALON Perform Range and offers a premi.. |
|||
Mold Temperature | 25.0 - 50.0 °C | 77.0 - 122 °F | |
Huntsman AVALON® 95 AE Thermoplastic Polyurethane Introduction: AVALON 95 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Sumitomo Chemical ESPOLEX® 3255 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Sumitomo Chemical ESPOLEX® 3675 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Sumitomo Chemical ESPOLEX® UT461A Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis BF335SA Polypropylene Copolymer BF335SA is a polypropylene copolymer intended for injection molding. This material has a very high impact strength while maintaining good stiffness, gives a good surface quality and is
easy to proc.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis Daplen™ ED117AE Polypropylene TPO Compound Daplen™ ED117AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis Daplen™ EF261AI Polypropylene TPO Compound Daplen™ EF261AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis Xmod™ GD301FE Polypropylene, Glass Fiber Reinforced Xmod™ GD301FE is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also a.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Eurostar Starpylen M1000-BK1A987 PP, Carbon Black Starpylen M1000-BK1A987 is a high carbon black load PP resinInformation provided by Eurostar. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Eurostar Starpylen MF007AS PP, Glass Fiber Filled, Injection Molded Starpylen MF007AS is a Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 10.0 - 50.0 °C | 50.0 - 122 °F | Injection |
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Mold Temperature | 10.0 - 50.0 °C | 50.0 - 122 °F | Injection |
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom SLOVALEN PQ 51 N Polypropylene Homopolymer, Modified with Elastomer, Impacted FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis Xmod™ MC55T1 Polypropylene Compound 10% Mineral Filled Xmod MC55t1 is a 10% mineral filled grade based on HCPP intended for injection molding. Xmod has been developed especially for the car industry, to be used in interior parts. XMod offers very good .. |
|||
Mold Temperature | 40.0 - 50.0 °C | 104 - 122 °F | |
Supreme Petrochem SP 6605 Toughened Polystyrene Characteristics Excellent melt strength High stiffness Easy tearability Processing Extrusion Applications Suitable for thin film for candy wrap and window envelope Economic production of clear th.. |
|||
Mold Temperature | 10.0 - 50.0 °C | 50.0 - 122 °F | Injection Molding |
Polimeri Europa Edistir N 1910 Polystyrene Very easy flow general purpose polystyrene. Used for injection of thin-wall, multi-cavity, very fast-cycle mouldings and for sheet extrusion in glossy capping of HIPS and in blend with HIPS or clear.. |