Taiwan PU Corporation TPU-C85 General Grade, Calender Molding Polyester Base TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Taiwan PU Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation TPU-C85 General Grade, Calender Molding Polyester Base TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Calender MoldingInformation provided by Taiwan PU Corporation.
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
Tensile Strength at Break 23.54 MPa
3414 psi
Elongation at Break 900 %
900 %
100% Modulus 0.00490 GPa
0.711 ksi
300% Modulus 0.00490 GPa
0.711 ksi
Resilience 45
45
%, Impact Resilience
Taber Abrasion, mg/1000 Cycles 20
20
Processing Properties Metric English Comments
Feed Temperature 170 °C
338 °F
Middle Barrel Temperature 175 °C
347 °F
Compress zone
Front Barrel Temperature 180 °C
356 °F
Metering zone
Adapter Temperature 185 °C
365 °F
Die Temperature 185 °C
365 °F