Processing Properties Metric English Comments
Adapter Temperature 185 °C
365 °F
NatureWorks® Ingeo™ AW 240D Biopolymer for Food Serviceware
NatureWorks® PLA polymer AW 240D is a thermoplastic resin derived from annually renewable resources. PLA polymer 2003D processes easily on conventional extrusion equipment. Specifically designed ..
Adapter Temperature 185 - 200 °C
365 - 392 °F
Petroquimica Triunfo Trithene® TS 7003 LDPE - High Strength Film
The Trithene TS 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily proc..
Adapter Temperature 185 - 285 °C
365 - 545 °F
Average value: 224 °C Grade Count:4
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported ..
Adapter Temperature 185 - 205 °C
365 - 401 °F
Petroquimica Triunfo Trithene® TX 7003 LDPE - Heavy Duty and Industrial Film
The Trithene® TX 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and environmental stress cracking resistance (ESCR). Additionally, this product..
Adapter Temperature 185 °C
365 °F
Huntsman IROGRAN® A 75 P 4655 N TPU-Polyester
Introduction: IROGRAN A 75 P 4655 N is a black colored polyether based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 75 P 4655 N is a part of the HUNTSMAN injecti..
Adapter Temperature 185 - 205 °C
365 - 401 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1030D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Adapter Temperature 185 - 195 °C
365 - 383 °F
Extrusion
Huntsman IROGRAN® A 87 P 4946 TPU-Polyester
Introduction: IROGRAN A 87 P 4946 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 87 P 4946 is part of the HUNTSMAN technical ext..
Adapter Temperature 185 °C
365 °F
Taiwan PU Corporation TPU-C85 General Grade, Calender Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Calender MoldingInformation provided by Taiwan PU Corporation.
Adapter Temperature 185 °C
365 °F
Taiwan PU Corporation TPU-CH85 High Hydrolysis Resistance, Calender Molding Polyether Base TPU
Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Calender MoldingInformation provided by Taiwan PU Corporation.
Adapter Temperature 185 °C
365 °F
Taiwan PU Corporation TPU-EH80 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU
Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Extrusion MoldingInformation provided by Taiwan PU Corporation.
Adapter Temperature 185 °C
365 °F
Taiwan PU Corporation TPUI-E80 General Grade, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
Adapter Temperature 185 °C
365 °F
Taiwan PU Corporation TPUI-L75 Low Temperature Resistance, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
Adapter Temperature 185 °C
365 °F
SK Chemicals SKYTHANE® CR180A Calendaring Series, Polyether Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Adapter Temperature 185 °C
365 °F
Lubrizol Estane® ZHF 78AT0 Thermoplastic Polyurethane, Flame Retardant
Type: Estane® ZHF 78AT0 NAT021 is a soft, polyether based, NHFR thermoplastic polyurethane (TPU) compound.Features: Soft, transparent, flame retardant.Uses: Wire and CableAvailable in Europe, Middl..
Adapter Temperature 185 °C
365 °F
Blown Film Coextrusion
DuPont™ Appeel® 72D799 Sealing Resin
DuPont™ Appeel® 72D799 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDP..
Adapter Temperature 185 °C
365 °F
Blown Film Coextrusion
DuPont™ Appeel® 72D811 Sealing Resin
DuPont™ Appeel® 72D811 resin is designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDPE, LDPE, EVA, and Ion..
Adapter Temperature 185 °C
365 °F
Blown Film Coextrusion
DuPont™ Bynel® 30E753 Anhydride Modified Ethylene Vinyl Acetate
BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Adapter Temperature 185 °C
365 °F
Blown Film Coextrusion
DuPont™ Bynel® 41E755 Anhydride Modified LLDPE
BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi..
Adapter Temperature 185 °C
365 °F
Blown Film Extrusion
DuPont™ Elvaloy® AC 1330 Ethylene Methyl Acrylate
Elvaloy® AC 1330 is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® A..
Adapter Temperature 185 °C
365 °F
Blown Film Coextrusion
DuPont™ Elvax® 3128-1 Ethylene Vinyl Acetate
DuPont™ Elvax® 3128-1 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® ..
Adapter Temperature 185 °C
365 °F
Blown Film Coextrusion
DuPont™ Nucrel® 30705 Ethylene Acrylic Acid
Nucrel® 30705 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethyle..
Adapter Temperature 185 °C
365 °F
Blown Film Coextrusion
DuPont™ Surlyn® E185SB Ionomer Resin
Surlyn® E185SB is an ionomer of an acid copolymer resin. It is designed for coextrusion with high-density polyethylene in peelable seals applications. It can be used in extrusion equipment designed..
Adapter Temperature 185 °C
365 °F
Equate EFDC-7087 LLDPE Film Extrusion Resin
EFDC-7087 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from EFDC-7087 have good toughness, high tensile strength and outstanding puncture resistance. EFDC-..
Adapter Temperature 185 - 190 °C
365 - 374 °F
Equate EMDA-6200 HDPE Blow Molding Resin
EMDA-6200 grade is a high-density polyethylene copolymer resin designed for blow molding small to medium size bottles. It can be used on intermittent as well as continuous blow molding machines for ..
Adapter Temperature 185 °C
365 °F
Blown Film Coextrusion
DuPont™ Surlyn® 1706 Zinc Ionomer
Surlyn® 1706 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t..
Adapter Temperature 185 °C
365 °F
Blown Film Coextrusion
DuPont™ Surlyn® 1707 Sodium Ionomer
Surlyn® 1707 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t..
Adapter Temperature 185 °C
365 °F
Blown Film Coextrusion
DuPont™ Surlyn® 1825 Zinc Ionomer
Surlyn® 1825 is available for use in conventional blown, cast film, sheet extrusion and coextrusion equipment designed to process polyethylene and ethylene copolymer type resins. SURLYN® 1825 comp..
Adapter Temperature 185 °C
365 °F
Blown Film Coextrusion
DuPont™ Surlyn® 2601B Sodium Ionomer
Surlyn® 2601B is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer ..
Adapter Temperature 185 - 235 °C
365 - 455 °F
Average value: 205 °C Grade Count:5
Overview of materials for Ionomer, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..
Adapter Temperature 185 °C
365 °F
5, Extrusion
Lubrizol Estane® ZHF 80AT3 Thermoplastic Polyurethane, Flame Retardant
Type: Estane® ZHF 80AT3 NAT 022 is an 80A non halogen, flame retardant, aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Transparent spherical pelletsFeatures: Zero halogenUses..
Copyright © lookpolymers.com All Rights Reserved