Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Taiwan Sheen Soon Sheenthane® A9830 Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP
Manufacturer Taiwan Sheen Soon Co. Ltd.
Trade Name Sheenthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan Sheen Soon Sheenthane® A9830 Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 96 - 100
96 - 100
Tensile Strength 29.4 MPa
4270 psi
Elongation at Break 500 %
500 %
100% Modulus 0.01273 GPa
1.846 ksi
300% Modulus 0.0196 GPa
2.84 ksi
Processing Properties Metric English Comments
Processing Temperature 190 - 220 °C
374 - 428 °F