Polymer Property : 100% Modulus = 1.846 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.01273 GPa
1.846 ksi
Taiwan Sheen Soon Sheenthane® A9313H Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
100% Modulus 0.01273 GPa
1.846 ksi
Taiwan Sheen Soon Sheenthane® A9315E Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD.
100% Modulus 0.01273 GPa
1.846 ksi
Taiwan Sheen Soon Sheenthane® A9660 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
100% Modulus 0.01273 GPa
1.846 ksi
Taiwan Sheen Soon Sheenthane® A9612K Film Grade Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD.
100% Modulus 0.01273 GPa
1.846 ksi
Taiwan Sheen Soon Sheenthane® A9830 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.