Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Taiwan Sheen Soon Sheenthane® AS-632L TPU for PU Adhesive

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP
Manufacturer Taiwan Sheen Soon Co. Ltd.
Trade Name Sheenthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan Sheen Soon Sheenthane® AS-632L TPU for PU Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Hydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations, furniture, spraying, and fire hose co-extrusion.Information provided by Taiwan Sheen Soon Co., LTD.
Physical Properties Metric English Comments
Viscosity 800 - 1200 cP
800 - 1200 cP
15% solids in MEK
Mechanical Properties Metric English Comments
Peel Strength 4.08 - 6.12 kN/m
23.3 - 34.9 pli
Initial (5 min.) PVC vs. PVC
Descriptive Properties Value Comments
Activation temperature (°C) 55-65
Heat Resistance, mm 25
70°C, PVC vs PVC
Max. Toluene in Solvents (%) 25-30
Tack Time, min 25 ~ 50
PVC vs PVC