Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 800 - 1500 cP @Temperature 23.9 °C |
800 - 1500 cP @Temperature 75.0 °F |
|
TSE Industries EcoWIND® 200 Polyurethane Resin Filament Winding
(discontinued **) TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Viscosity | 800 cP | 800 cP | ASTM D2293 |
Fibre Glast Saf-T-Poxy 2410 / 2184 Epoxy
(discontinued **) Information provided by Fibre Glast Developments Corporation. |
|||
Viscosity | 800 - 1700 cP | 800 - 1700 cP | |
Huntsman Araldite AER 4100 N80 Brominated Resin Weight per Epoxide (EEW, g/eq) 330 to 370. Max color is 5.Comments/Applications: Brominated epoxy resin solution in MEK, designed for use in high density multilayer circuit boards exhibiting high g.. |
|||
Viscosity | 800 - 1600 cP | 800 - 1600 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1102 J (SBS) Liner Block Copolymer Description: Kraton D1102 J is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Japan in the physical form(s) identified below in the.. |
|||
Viscosity | 800 cP | 800 cP | Solution Viscosity; ASTM D455 |
Solvay Specialty Polymers Veradel® 3100P Polyethersulfone (PESU) Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with oth.. |
|||
Viscosity | 800 cP | 800 cP | Solution Viscosity; ASTM D455 |
Solvay Specialty Polymers Virantage® VW-10300 P, FP & SFP Polyethersulfone (PESU) Virantage® VW-10300 polyethersulfone (PESU) is a non-functionalized, high-temperature sulfone polymer powder. Three grades are offered: Virantage® VW-10300P, Virantage® VW-10300FP, and Vira.. |
|||
Viscosity | 800 cP @Temperature 25.0 °C |
800 cP @Temperature 77.0 °F |
|
Struktol STRUKSILON 8023 Silicone Stabilizer for PU-Rigid Foam STRUKSILON 8023 is a universal stabilizer for polyurethane rigid foams. It is especially recommended for the use in poor in place and roof sprayfoam applications.Applications: Information provided b.. |
|||
Viscosity | 800 - 1700 cP | 800 - 1700 cP | |
Solvay RHODOLINE® DF-665 Surfactant Description: Highly efficient mineral oil based defoamers for flat to gloss paints, quick process foam know down and high in-can persistency.Identification: OIL BASE DEFOAMERAvailable in: North Amer.. |
|||
Viscosity | 800 cP @Temperature 23.0 °C |
800 cP @Temperature 73.4 °F |
|
Master Bond EP29LP Low Exotherm, Low Viscosity Two Component Epoxy System Master Bond Polymer System EP29LP is a two component high performance epoxy resin system featuring low viscosity, long pot life and low exotherm. As an adhesive this versatile material will form bon.. |
|||
Viscosity | 800 cP | 800 cP | dynamic |
Dow Corning FG-10 ANTIFOAM EMULSION 10 percent active, food-grade silicone emulsion designed to control foam in aqueous systems.Information provided by Dow Corning |
|||
Viscosity | 800 cP | 800 cP | dynamic |
Dow Corning SE 1880 One-part, transparent gel, heat cure, low temperature capable.Information provided by Dow Corning |
|||
Viscosity | 800 cP | 800 cP | Dynamic |
Dow Corning SYL-OFF® PMCPSL 10 Release Modifier Olefin-free; low viscosityInformation provided by Dow Corning |
|||
Viscosity | 800 cP | 800 cP | Dynamic |
Dow Corning SYL-OFF® PMCPSL 50 Release Modifier Information provided by Dow Corning |
|||
Viscosity | 800 cP | 800 cP | dynamic |
Dow Corning SYL-OFF® SL 50 RELEASE MODIFIER Information provided by Dow Corning |
|||
Viscosity | 800 cP @Temperature -25.0 °C |
800 cP @Temperature -13.0 °F |
Cold Crank |
ChevronTexaco 4R Unconventional Base Oil FeaturesChevron Unconventional Base Oils (UCBOs) are all hydroprocessed, highly refined paraffinic base oils of exceptional performance and purity.Relative to conventional hydroprocessed and solvent.. |
|||
Viscosity | 800 cP @Temperature 160 °C |
800 cP @Temperature 320 °F |
Melt; ETM 22-31 |
ExxonMobil ESCOREZ™ 5400 Petroleum Hydrocarbon Resin Light colored cycloaliphatic hydrocarbon resin. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, natural rubber, synthetic polyisoprene, poly.. |
|||
Viscosity | 800 cP @Temperature 25.0 °C |
800 cP @Temperature 77.0 °F |
|
Cytec (Conap) RN-1000 / EA-117 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Viscosity | 800 - 1600 cP @Temperature 23.0 °C |
800 - 1600 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 302-3M Optically Transparent Epoxy Product Description: EPO-TEK® 302-3M is a two component epoxy used for optical, medical, fiber optic, and semiconductor applications. The epoxy is good for adhesive joining, sealing, potting, or as.. |
|||
Viscosity | 800 - 1200 cP @Temperature 23.0 °C |
800 - 1200 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® CF6-2 High Temperature Epoxy Product Description: EPO-TEK® CF6-2 is a two component, high temperature and high Tg epoxy designed for fiber optic packaging. Advantages & Application Notes: The low viscosity nature allows for wi.. |
|||
Viscosity | 800 - 1600 cP @Temperature 23.0 °C |
800 - 1600 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® E4110 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E4110 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although other.. |
|||
Viscosity | 800 - 1200 cP | 800 - 1200 cP | |
Epoxyset Epoxibond EB-119M Unfilled Epoxy Adhesive A two-component,unfilled, low viscosity, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by.. |
|||
Viscosity | 800 cP | 800 cP | A Side |
ACC EP EF EPI Engineered Polymers Extra Flex Polyurea EP EF, Extra Flex Polyurea, “Powered by Reactamine® Technology, is a two component 100% solid Polyurea, with superior performance in industrial applications. EP EF displays extremely fast cure tim.. |
|||
Viscosity | 800 cP | 800 cP | "B" component |
ACC QLE 1035 QSI Quantum Silicones 38 Durometer Addition Cure Elastomer for Coating QLE 1035 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: .. |
|||
Viscosity | 800 - 1600 cP | 800 - 1600 cP | |
Beijing Ranger Chem SM-815CA Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 800 - 1000 cP | 800 - 1000 cP | Mixed Viscosity |
Aremco Corr-Paint™ CP2070 High Temperature Protective Coating Novolac-Epoxy, Pigment Only Filled Two part, novolac-epoxy with exceptional abrasion adn corrosion resistance for continuous operations to 300°F (150°C) and intermittent use to 400°F (204°C). |
|||
Viscosity | 800 - 1000 cP @Shear Rate 50.0 1/s, Temperature 25.0 °C |
800 - 1000 cP @Shear Rate 50.0 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2080815P1 Silver Flexographic Ink Silver conductor ink specifically designed for printing on to polymeric or paper substrates using flexographic printing. Ink can be printed at speeds up to 20m/min, with good line definition and go.. |
|||
Viscosity | 800 - 1500 cP @Temperature 23.0 °C |
800 - 1500 cP @Temperature 73.4 °F |
|
Master Bond UV15-7SP4DC One Component, Dual Cured, Flexible UV System Master Bond Polymer System UV15-7SP4DC is a one component, optically clear, dual cured flexible UV and/or heat curable polymer system with extended service capability of -80°F to +250°F. It cures .. |
|||
Viscosity | 800 cP | 800 cP | |
KKPC KOSYN KSL 341 Styrene-Butadiene Latex Styrene-Butadiene LatexCharacteristics: KOSYN KSL 300 series is a Styrene-Butadiene Latex. KSL 341 has big granules and high concentration. It shows excellent processability in rubber sponge produc.. |