Techmer ES Elastoblend® PA6 IM 811 HS L (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Heat Stabilized , Nylon 6, Impact Grade
Manufacturer Techmer ES
Trade Name Elastoblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Elastoblend® PA6 IM 811 HS L (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedTPCI# 6109102Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Water Absorption 1.5 %

@Time 86400 sec
1.5 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0080 cm/cm

@Thickness 3.17 mm
0.0080 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Strength 51.7 MPa
7500 psi
ASTM D790
Flexural Modulus 0.862 GPa
125 ksi
ASTM D790
Izod Impact, Notched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256