Techmer ES Electrafil® DB-5/SS/10 Polycarbonate, 10% Stainless Steel Fiber (dry blend)

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Stainless Steel Fiber
Manufacturer Techmer ES
Trade Name Electrafil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrafil® DB-5/SS/10 Polycarbonate, 10% Stainless Steel Fiber (dry blend).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm

@Thickness 3.17 mm
0.0040 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 64.1 MPa
9300 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Yield Strength 96.5 MPa
14000 psi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 1.00 - 10.0 ohm-cm
1.00 - 10.0 ohm-cm
ASTM C611
Surface Resistance 0.10 - 1.0 ohm
0.10 - 1.0 ohm
ASTM D257