Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Water Absorption 0.11 %
0.11 %
24 Hrs; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength at Break 89.6 MPa
13000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 131 MPa
19000 psi
ASTM D790
Flexural Modulus 4.21 GPa
610 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
260 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 100 - 1000 ohm
100 - 1000 ohm
ASTM D648