Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
PolyOne Edgetek® PS-20CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
PolyOne Stat-Tech™ PS-18CF/000 CM Black Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinu Preliminary Data SheetDescription/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
PolyOne Edgetek® ATH-20CF/000 Acetal-Homopolymer, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedElectrically ConductivePolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
PolyOne Lubri-Tech™ PI-30CF/15T Polyetherimide (PEI), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 800 - 1000 ohm | 800 - 1000 ohm | prints from standard 140/31 screen |
Heraeus Cleviosâ„¢ S HT Antistatic/Conductive Polymer Coating for Screen Printing Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as a paste designed for application by silk screen printing to be used for transparent conductive devices. Cleviosâ„¢ S HT grade .. |
|||
Surface Resistivity per Square | 100 - 1000 ohm | 100 - 1000 ohm | ASTM D648 |
Techmer ES Electrafil® J-1305/CF/30/TF/15 BK PPS |
|||
Surface Resistivity per Square | 100 - 1000 ohm | 100 - 1000 ohm | ASTM D648 |
Techmer ES Electrafil® J-1305/CF/30/TF/15 NAT PPS |
|||
Surface Resistivity per Square | 100 - 1000 ohm | 100 - 1000 ohm | ASTM D648 |
Techmer ES Electrafil® NY-3/EC BK PA6 |
|||
Surface Resistivity per Square | 100 - 1000 ohm | 100 - 1000 ohm | ASTM D648 |
Techmer ES Plaslube® J-1/CF/15/TF/20 NAT PA66 |
|||
Surface Resistivity per Square | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
PolyOne Edgetek® AM-30CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
PolyOne Lubri-Tech™ AM-30CF/15T Polyphthalamide (PPA), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |