Techmer ES HiFill FR® PP CO FR-N

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Flame Retardant , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Techmer ES
Trade Name HiFill FR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill FR® PP CO FR-N.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFeatures: Flame Retardant, High Impact Resistance and CopolymerInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.010 cm/cm

@Thickness 3.17 mm
0.010 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
Elongation at Yield 350 %
350 %
ASTM D638
Flexural Yield Strength 22.8 MPa
3300 psi
ASTM D790
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
Izod Impact, Notched 3.20 J/cm

@Thickness 3.17 mm
6.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
220 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C
180 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 17.7 kV/mm
450 kV/in
Method A (Short-Time); ASTM D149