Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® PA6/6 GF60 HS L BK 60% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 60% Glass Fiber Filled , Nylon 66, Heat Stabilized
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA6/6 GF60 HS L BK 60% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Number: E157318Appearance: BlackTPCI# 7859101Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
ASTM D792
Water Absorption 0.35 %

@Time 86400 sec
0.35 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Yield 207 MPa
30000 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Flexural Strength 331 MPa
48000 psi
ASTM D790
Flexural Modulus 19.3 GPa
2800 ksi
ASTM D790
Izod Impact, Notched 2.08 J/cm

@Thickness 3.17 mm
3.90 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 23.4 µm/m-°C
13.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 257 °C
495 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
ASTM D257
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
ASTM D257
Dielectric Strength 19.7 kV/mm
500 kV/in
Method A (Short-Time); ASTM D149
Users viewing this material also viewed the following: