Material Notes:
Plaslube glass fiber reinforced, polytetrafluoroethylene (PTFE) lubricated nylon 66 grades offer an excellent balance of wear and friction performance and mechanical strength. The addition of silicone to these products enhances the wear and friction performance of these grades. Typical applications include pulleys, wear slides, cams, gears and high strength bearings.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Water Absorption 0.70 %
0.70 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 169 MPa
24500 psi
ASTM D638
Flexural Yield Strength 245 MPa
35500 psi
ASTM D790
Flexural Modulus 8.62 GPa
1250 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm

@Thickness 3.17 mm
2.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Coefficient of Friction, Dynamic 0.27
0.27
Coefficient of Friction, Static 0.22
0.22
K (wear) Factor 50.4 x 10-8 mm³/N-M
25.0 x 10-10 in³-min/ft-lb-hr
Thrust washer at 2000 PV
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 257 °C
495 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 251 °C
484 °F
ASTM D648