Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
PolyOne Nymax™ GF 1200 33 Red 31 A Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
PolyOne Nymax™ GF 924 33 UV Black 108 Polyamide 66 (Nylon 66) Property data for molded test bars: Dry as MoldedInformation provided by PolyOne |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Nylene® 9633 , 33% Glass Reinforced Nylon 6,6/6 Description: Nylene® 9633 is a 33% glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resou.. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Niche Polymer PA6GF33BK Nylon 6, 33% Glass Fiber Filled Information provided by Niche Polymer |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N2233HL BK Nylon 6 Available in North America Filler: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Proces.. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | Tangent, 0.125 in; ASTM D790 |
Matrixx Group 80S7301 30% Glass Reinforced PET
(discontinued **) Data provided by The Matrixx Group, formerly RePlas. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ISO 178, ASTM D790 |
Nilit Nilamid B G6 FR C4 30% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G6 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ.. |
|||
Flexural Modulus | 8.63 GPa | 1250 ksi | ASTM D790 |
Gromax PBT 5130-104 30% Glass Fiber Filled CCP Halogen-free PBT, Black. PBT flame-retarded glass fiber 30% reinforced injection molding gradeCharacteristics:Excellent electrical property Excellent temperature resistance, high heat distortion.. |
|||
Flexural Modulus | 8.63 GPa | 1250 ksi | 5 mm/min; ISO 178 |
Gromax BFG30-EN03N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 8.61 GPa | 1250 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP QFP36 PA 6/10 (Asia Pacific) LNP LUBRICOMP* QFP36 is a compound based on Nylon 6/10 resin containing Silicone, PTFE, Glass Fiber. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® AG-330 Polyethersulfone (PESU), 30% Glass Fiber Veradel® AG-330 is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF33 L NAT004 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: Natural ColorTPCI# 9411102Informatio.. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF33 L RD079 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: RedInformation provided by TP Compos.. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK (Asia Pacific) LNP* Thermocomp* LF005 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF WF006I PBT LNP THERMOTUF* WF006I is a compound based on PBT containing 30% Glass Fiber. Added features of this material include: High Impact. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ASTM D790 |
Plenco 00755 Melamine-Phenolic, Granular, Transfer Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ASTM D790 |
Plenco 4527 Phenolic, Granular, Injection Molded PLENCO 04527 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength, and resistance to cracking in a wet-dry environment. UL recognized under.. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ASTM D790 |
Plenco 4309 Phenolic, Nodular, Injection Molded PLENCO 04309 is a heat resistant, glass reinforced phenolic molding compound offering improved mechanical strength and electrical strength properties. UL recognized under component file E40654. 0430.. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ISO 178 |
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Dry) Ultramid B3EG6 BK00564 is a 30% glass fiber reinforced, pigmented black injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ISO 178 |
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Dry) Information provided by BASF |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 421 Polyester - PBT, Glass/Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ASTM D790 |
Ashley Polymers Ashlene® 67MG Nylon 66, Glass/Mineral reinforced A glass/mineral reinforced Nylon 66 designed for high strength and dimensional stability.Data provided by the manufacturer |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ISO 178 |
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Dry) Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Teknor Apex Chemlon® 133 G Nylon 66, 33% Short Glass Fiber Filled Notes: Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets FMVSSInformation Provided by Teknor Apex |