Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Plaslube® J-50/20/TF/10 Polycarbonate, 20% GFR, 10% PTFE

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Glass + PTFE Filled
Manufacturer Techmer ES
Trade Name Plaslube®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plaslube® J-50/20/TF/10 Polycarbonate, 20% GFR, 10% PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Water Absorption 0.11 %
0.11 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 103 MPa
15000 psi
ASTM D638
Flexural Yield Strength 159 MPa
23000 psi
ASTM D790
Flexural Modulus 5.86 GPa
850 ksi
ASTM D790
Izod Impact, Notched 1.87 J/cm

@Thickness 3.17 mm
3.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
290 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved