Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Water Absorption 1.0 %
1.0 %
24 Hrs; ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 58.6 MPa
8500 psi
ASTM D638
Flexural Strength 103 MPa
15000 psi
ASTM D790
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °C
170 °F
ASTM D648