Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Plastiblend® PC/PBT IM 1799 BK

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Techmer ES
Trade Name Plastiblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plastiblend® PC/PBT IM 1799 BK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Thickness 3.17 mm
0.0040 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 16 g/10 min

@Load 5.00 kg,
Temperature 265 °C
16 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 120 %
120 %
ASTM D638
Flexural Yield Strength 95.1 MPa
13800 psi
ASTM D790
Flexural Modulus 2.55 GPa
370 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
3.00 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
7.47 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
14.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Dart Drop, Total Energy 6.21 J

@Temperature -28.9 °C
4.58 ft-lb

@Temperature -20.0 °F
ASTM D3763
6.33 J

@Temperature 22.8 °C
4.67 ft-lb

@Temperature 73.0 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 81.0 µm/m-°C
45.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 118 °C
245 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB