Material Notes:
Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite Features: LubricatedUnoriented Magnetic:Residual Induction, BR: 1100 GaussCoercive Force, Hc: 750 OerstedsIntrinsic Coercive Force, Hc: 2400 OerstedsMaximum Energy Produce, Bh max: 0.2 Mega Gauss OerstedsOriented Magnetic:Residual Induction, BR: 1500 GaussCoercive Force, Hc: 1050 OerstedsIntrinsic Coercive Force, Hc: 2300 OerstedsMaximum Energy Produce, Bh max: 0.4 Mega Gauss OerstedsInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 3.35 g/cc
0.121 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.1 MPa
6400 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Flexural Strength 75.8 MPa
11000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm
0.600 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 36.0 µm/m-°C
20.0 µin/in-°F
ASTM D696
Melting Point 271 °C
520 °F
Deflection Temperature at 0.46 MPa (66 psi) 260 °C
500 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 249 °C
480 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
ASTM D257