Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 36.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EM2212 PC Automotive interiors. 10% glass-reinforced. Increased stiffness/structural ridigity. High modulus/ductile. Foamed skin instrument panel uses also. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
PolyOne Edgetek® AS-20GF/000 Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
LG Chemical LUMID HI2152A(W) PA6+GF15%, High Impact Feature: Injection Molding, PA6+GF15%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 and 5VA listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC LNP* Lubricomp* Lexan_LF1510A compound is a 10% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6 GF30 IM BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6 GF40 IM HS UV RD 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6 GF43 IM L BKN 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2110EPR PEI 10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2210EPR PEI (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2212EPR PEI (Asia Pacific) 20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
20.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP WFL34 PBT LNP LUBRICOMP* WFL34 is a compound based on PBT resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6 GF25 FR HS L 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 GF25 FR BK 25% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedAppear.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA4/6 0206 Availability: North AmericaForms: PelletsFeatures: High Specific Gravity and Thermally ConductiveInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedUL File Number: E157318Appearanc.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 LGF30 HS L 12mm 30% Glass/Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedIn.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
20.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF006EUC PA 66 LNP* THERMOCOMP* RF006EUC is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include Easy Molding, UV Stabilized. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
20.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP YF005 POLYESTER ELASTOMER LNP* THERMOCOMP* YF005 is a compound based on Polyester Elastomer resin containing 25% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Heat Stabilized Polyamide 66 Minlon 10B40HS1 BK061 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
20.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam RF0052E PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam RF0052E is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® DP T 7140 LDS 000000 PBT + PET, 44% Mineral + L227Glass Fiber
(discontinued **) PET+PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimension stability |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6 GF25 FR 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Flame RetardantFeatures: Flame Retardant UL File Number: E157318Processing Met.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PPO/HIPS MM20 IM FR 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightAdditive: Impact Modifier Features: Flame Retardant and Impact ModifiedInformation provided by TP C.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA4/6 GF30 FR HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Flame Retardant and Lu.. |