Material Notes:
Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite Features: LubricatedInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 3.28 g/cc
0.118 lb/in³
ASTM D792
Water Absorption 0.20 %

@Time 86400 sec
0.20 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.010 cm/cm

@Thickness 3.17 mm
0.010 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 48.3 MPa
7000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 84.8 MPa
12300 psi
ASTM D790
Flexural Modulus 13.1 GPa
1900 ksi
ASTM D790
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 1.87 J/cm

@Thickness 3.17 mm
3.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 32.4 µm/m-°C
18.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 204 °C
400 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
ASTM D257