Techmer ES Statiblend® PA6/6 GF10 BK 10% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled , Nylon 66, Conductive
Manufacturer Techmer ES
Trade Name Statiblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Statiblend® PA6/6 GF10 BK 10% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: LubricantFeatures: Conductive and LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Water Absorption 0.80 %

@Time 86400 sec
0.80 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Thickness 3.17 mm
0.0060 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D785
Tensile Strength, Yield 85.5 MPa
12400 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Strength 121 MPa
17500 psi
ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 54.0 µm/m-°C
30.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 232 °C
450 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+8 - 1.00e+11 ohm-cm
1.00e+8 - 1.00e+11 ohm-cm
ASTM D257
Surface Resistance 1.00e+8 - 1.00e+11 ohm
1.00e+8 - 1.00e+11 ohm
ASTM D257