Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 121 MPa | 17600 psi | ASTM D-790 |
Plaskolite Optix® CA - 75 OG General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Flexural Strength | 121 MPa | 17600 psi | ASTM D-790 |
Plaskolite Optix® CA - 75 UVT General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
PolyOne LubriOne™ PC-20CF/15T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
Parker Chomerics PREMIER™ A220-ST EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
Polymer Resources TP-FRG7.5 Polybutylene Terephthalate, 7 1/2 % Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 7 1/2 % Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Flexural Strength | 121 MPa | 17500 psi | 1.3 mm/min; ASTM D790 |
PolyOne Edgetek® COC BLEND-15GF Natural Cyclic Olefin Copolymer (COC) Information provided by PolyOne |
|||
Flexural Strength | 121 MPa | 17500 psi | |
Poco Graphite EDM-4 EDM Graphite POCO's EDM-4 is our premier offering in the Ultrafine classification. This highly isotropic grade combines strength with moderate hardness, yielding superior electrode fabrication characteristics. T.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
Gharda Chemicals Gafone™ T6500 Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional Properties Transparent High Mechanical Properties Good Electrical Properties High Tg of 270°C and expected Continuous Use Temperature of 220°C App.. |
|||
Flexural Strength | 121 MPa | 17500 psi | |
Cookson Group Plaskon® 3200LS Mineral Filled Novolac Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability under very stringent testing. This material is designed to minimize stress on the encapsulated .. |
|||
Flexural Strength | 121 MPa | 17500 psi | ISO 178 |
Premix Premi-Glas® 1265 VE 1265-VE (Compression Molded) Glass Reinforced Vinyl Ester TMC
(discontinued **)< Description: Premi-Glas® 1265 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injecti.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Flexural Strength | 121 MPa | 17500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP WF002 PBT LNP* THERMOCOMP* WF002 is a compound based on PBT containing 10% Glass Fiber. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Strength | 121 MPa | 17500 psi | 21% Glass Spray-up Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Flexural Strength | 121 - 128 MPa | 17500 - 18500 psi | ASTM D790 |
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon Offering improved tensile, compressive and flexural properties over conventional unfilled cast nylon, NYCAST® GF (Glass Filled)-30% provides increased load bearing characteristics and is the choice.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
Asahi Kasei Thermylene® P6-40FG-0700 40% Glass Fiber Reinforced, High Impact Information provided by Asahi Thermofil |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 105 Polypropylene, Glass Reinforced, Chemically Coupled, Impact Modified Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Flexural Strength | 121 MPa | 17600 psi | ASTM D-790 |
Plaskolite Optix® CP - 75 HID General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Flexural Strength | 121 MPa | 17600 psi | ASTM D-790 |
Plaskolite West Optix® CA - 75 OG General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |