Technetics Group PLASTOLON™ Low Density PTFE Tape  (Unverified Data**)

Category Polymer , Tape , Thermoplastic , Fluoropolymer , PTFE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Technetics Group PLASTOLON™ Low Density PTFE Tape  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Technetics Group (formerly Plastomer Technologies)
Physical Properties Metric English Comments
Specific Gravity 0.700 g/cc
0.700 g/cc
Thickness 76.2 - 254 microns
3.00 - 10.0 mil
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 10.3 MPa
>= 1500 psi
Elongation at Break >= 70 %
>= 70 %
Descriptive Properties Value Comments
Available Colors Natural
Laser Printable No
Width, in 1/4-4
Copyright © lookpolymers.com All Rights Reserved