Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 10.3 - 14.5 MPa | 1490 - 2100 psi | ASTM D638-95 |
Multibase Multi-Flex® TPO 1047-4107 Passed impact resistance 3.4J at -30°C; ASTM GM 9032 P. This product is UV stabilized for automotive applications, like fender guards and airbags.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1490 psi | post cured- 4 hours at 204°C |
Multibase SILASTIC® C7-4550 TBPB Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1490 psi | ASTM D638 |
ExxonMobil Escorene® LD-411 LDPE Power Cable Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable polyethylene homopolymer designed as an electrical grade base resin especially suitable for Henschel blending.Applications: A base r.. |
|||
Tensile Strength, Ultimate | >= 10.3 MPa | >= 1500 psi | |
Technetics Group PLASTOLON™ Low Density PTFE Tape
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1490 psi | ASTM D3574E |
Mearthane Durethaneâ„¢ F DF-225A Closed Cell Foam Polyurethane TDI backbone: ester.Shore 00 Hardness: 70Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient.. |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1490 psi | |
Kuraray HYBRAR® SC1 Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1500 psi | |
Sylvin Technologies 8600-60 Clear PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1500 psi | |
Sylvin Technologies 8999-75 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1500 psi | |
Sylvin Technologies 9600-60 Clear PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1500 psi | |
Sylvin Technologies 9925-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1500 psi | |
Sylvin Technologies 9999-75 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1500 psi | |
Sylvin Technologies 9999-90 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1500 psi | ASTM D638 |
Westlake EC479AA Low Density Polyethylene WESTLAKE low-density polyethylene EC479 is recommended for use in the boardstock coating industry. This resin has low neck-in, good heat sealing properties, and good drawdown characteristics.Applica.. |
|||
Tensile Strength, Ultimate | 10.3 MPa @Treatment Temp. 150 °C, Time 605000 sec |
1490 psi @Treatment Temp. 302 °F, Time 168 hour |
Heat Aging; ASTM D 412/ASTM D 573 |
Zylog Neoplast® 180 C Thermoplastic Vulcanizate Neoplast 180 C is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, UV S.. |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1490 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8100 Polyolefin Elastomer Description: Engage® 8100 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide range of general purpose thermoplastic elastomer ap.. |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1490 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8107 Polyolefin Elastomer Description: Engage® 8107 polyolefin elastomer is a loose talc surface coated ethylene-octene copolymer. The talc is untreated and has a nominal 1µm particle size. This product offers the exceptio.. |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1500 psi | ASTM D638 |
Colorite Polymers Vinylbond 6527P-MD Grey 499 Compound Description: Vinylbond 6527P-MD Grey 499 is a flexible vinyl compound which offers excellent bonding to ABS, low gloss, and low fogging characteristics for use in automotive interior applications. T.. |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1490 psi | |
Dow HDPE 42047N High Density Polyethylene DOW HDPE 42047N resin is a narrow molecular weight distribution copolymer designed to combine high impact strength and environmental stress crack resistance with excellent processability over a wide.. |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1490 psi | |
Dow HDPE 65053N High Density Polyethylene DOW HDPE 65053N resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and rigidity with high impact strength. This resin has excellen.. |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1490 psi | |
Dow LDPE 4005M Low Density Polyethylene Data provided by Dow Chemical. |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1490 psi | DOWM 100789-LE90A |
Dow Tyrin® CM674 Elastomer Formulation FormulationTyrin® CPE Elastomer |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1500 psi | ASTM D412 |
Colorite Polymers CS1515GP Non Lead Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 10.3 MPa @Thickness 1.14 - 1.52 mm, Temperature 816 °C |
1490 psi @Thickness 0.0449 - 0.0598 in, Temperature 1500 °F |
|
AK Steel 409 Ferritic Stainless steel AK Steel 409 Stainless Steels are especially useful for applications where oxidation or corrosion protection beyond the capacity of carbon steel and some coated steels is needed. Current applicatio.. |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1500 psi | ASTM D412 |
Advanced Polymer Alloys DURACRYN 8060 NC/BK Thermoplastic Rubber Information provided by Advanced Polymer Alloys |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1500 psi | |
Colorite Polymers 5511 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
Tensile Strength, Ultimate | 10.3 MPa | 1500 psi | |
Colorite Polymers 5512 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Tensile Strength, Ultimate | 10.3 - 18.0 MPa | 1500 - 2610 psi | Average value: 14.1 MPa Grade Count:23 |
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum .. |
|||
Tensile Strength, Ultimate | 10.3 - 300 MPa | 1500 - 43500 psi | Average value: 31.7 MPa Grade Count:167 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |