Teknor Apex APEX® 80118-Y Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 80118-Y Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 60°C Insulation; RoHS Compliant Features: Good UV Resistance Uses: Cable Jacketing; InsulationAgency Ratings: UL 1063; UL 1581; UL 62; UL 83 Forms: Pellets Wire Types: TWInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 86
86
10 seconds; ASTM D2240
Tensile Strength at Break 17.6 MPa
2550 psi
ASTM D638
Elongation at Break 280 %
280 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Continuous Use; ASTM D794
Brittleness Temperature -28.0 °C
-18.4 °F
ASTM D746
Oxygen Index 23 %
23 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 3.46

@Frequency 1.00e+6 Hz
3.46

@Frequency 1.00e+6 Hz
ASTM D150
5.39

@Frequency 1000 Hz
5.39

@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.079

@Frequency 1.00e+6 Hz
0.079

@Frequency 1.00e+6 Hz
ASTM D150
0.089

@Frequency 1000 Hz
0.089

@Frequency 1000 Hz
ASTM D150
Descriptive Properties Value Comments
Appearance Opaque
Users viewing this material also viewed the following: