Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable JAC32A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WJJC340U Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Eastman 812A Polyethylene
(discontinued **) Polyethylene 812A is a natural low density material with a 200 melt index. This high-flow formulation is used for specialty injection molding applications in the medical market.Unless otherwise not.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Teknor Apex APEX® 3201-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Teknor Apex APEX® 3311-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Teknor Apex APEX® 3600-85NT Polyvinyl Chloride, Flexible Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: First Generation SeriesInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Teknor Apex APEX® 3700-90 Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Teknor Apex APEX® 65002 Polyvinyl Chloride, Flexible Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; Lead-free Uses: Communication Wire JacketingForms: Pellets Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 770; NEC Ar.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Teknor Apex APEX® 84137 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: Flame Retardant; Sunlight Resistant (720 hours) Uses: Cable Jacketing Agency Ratings: UL 62 Wire Types: SAE; SJTW; SPT-1; SPT-2; SPT-3; SRDT; STW; SVTForms: PelletsIn.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Teknor Apex HFFR 2006 Polyolefin, Halogen Free Notes: RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable Jacketing Agency Ratings: IEC Unspecified Rating; ICEA Un.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Teknor Apex MF 573 Polyvinyl Chloride, Flexible Film Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsInformation provided by Teknor Apex Company |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | |
Sylvin Technologies 6034-85 UV PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | |
Sylvin Technologies 6128-90 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | Temperature Retraction, TR-10 |
Dow Nordel® IP 4770R Heat Resistant Peroxide Compound FormulationNordel® IP 4770R |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Colorite Polymers 92-605 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PH 75/SN Flexible PVC, Transparent Extrusion Transparent and flexible sheets |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PH 76/A Flexible PVC, Transparent Extrusion Water pipes |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 7010/K Flexible PVC, Lead Free Pipes |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 835WA Wire & Cable Flexible PVC AWM for SPT, SJT and SVT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 10870 Wire & Cable Flexible PVC General purpose jacket compound recommended for 60C applications and also suited for 75C at a wall thickness of 30 mils and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corp.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 12860 Wire & Cable Flexible PVC 80C liquid tight conduit.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 18770 Moldings & Extrusions Flexible PVC General purpose 105C, clear jacketing compound recommended for 1/32" wall and larger. Exhibits excellent migration properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 22902 Coax & Telecom Flexible PVC Non-lead stabilized riser jacket recommended over PVC and FRHDPE primaries. Maximum service temperature rating of 75°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 6850 Moldings & Extrusions Flexible PVC Low gravity compound for extrusion and molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 873 Wire & Cable Flexible PVC 80°C rated, low migratory, oil resistant coil cord jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | |
AlphaGary GW 2403-1 VW1 105-LCF Flame Retardant Polyvinyl Chloride 105°C rated low temperature oil & sunlight resistant jacketing compound for tray cable application |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PK 7015/UV Flexible PVC, Lead Free Outdoor profiles anti-UV |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 22930 Coax & Telecom Flexible PVC Jacket compound suitable for riser applications when used with flame retardant PVC primaries. Maximum service temperature of 75°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 4441 Flexible PVC 85C non-lead stabilized wire harness. SAE J1128.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 8050 Flexible PVC, Lead Free Pipes and profiles |