Teknor Apex APEX® 94-A0098A-84 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 94-A0098A-84 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-Injection Molding Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
15 seconds; ASTM D2240
Tensile Strength, Yield 18.9 MPa
2740 psi
ASTM D412
Elongation at Break 350 %
350 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D746