Material Notes:
Features: Monprene® TPE gels are softer than the shore A range of hardness. Monprene® TPE gels are high strength and high flow elastomers that may be used in the overmolding processes on polyolefin substrates. Monprene® TPE gels are recommended for applications where very soft tactile feel and strength are required, such as cushions or padding between hard substrates and personal contact.Information Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.870 g/cc
0.870 g/cc
ASTM D792
Melt Flow 10.0 g/10 min

@Load 2.16 kg,
Temperature 125 °C
10.0 g/10 min

@Load 4.76 lb,
Temperature 257 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
ASTM D2240
Tensile Strength at Break 1.24 MPa
180 psi
ASTM D412
Tensile Strength, Yield 0.241 MPa

@Strain 300 %
35.0 psi

@Strain 300 %
ASTM D412
Elongation at Break 700 %
700 %
ASTM D412